Add to Cart
Ni70Cr30 is an austenitic nickel-chromium alloy suitable for temperature applications up to 1250°C. High chromium content (30% in average) provides very good life time, especially in the furnace applications.
Ni70Cr30 is characterized by high resistivity, good oxidation resistance, good ductility after use and excellent weldability. Alloy is not subject to “green rot” and is particularly well suited for reducing and oxidizing atmospheres.
Ni70Cr30 is used for electric heating elements in industrial furnaces. Typical applications are: electric and enamelling furnaces, storage heaters, furnaces and kilns with a changing atmospheres.
Performance material | Cr10Ni90 | Cr20Ni80 | Cr30Ni70 | Cr15Ni60 | Cr20Ni35 | Cr20Ni30 | |
Composition | Ni | 90 | Rest | Rest | 55.0~61.0 | 34.0~37.0 | 30.0~34.0 |
Cr | 10 | 20.0~23.0 | 28.0~31.0 | 15.0~18.0 | 18.0~21.0 | 18.0~21.0 | |
Fe | ≤1.0 | ≤1.0 | Rest | Rest | Rest | ||
Maximum temperature℃ | 1300 | 1200 | 1250 | 1150 | 1100 | 1100 | |
Meltiing point ℃ | 1400 | 1400 | 1380 | 1390 | 1390 | 1390 | |
Density g/cm3 | 8.7 | 8.4 | 8.1 | 8.2 | 7.9 | 7.9 | |
Resistivity | 1.09±0.05 | 1.18±0.05 | 1.12±0.05 | 1.00±0.05 | 1.04±0.05 | ||
μΩ·m,20℃ | |||||||
Elongation at rupture | ≥20 | ≥20 | ≥20 | ≥20 | ≥20 | ≥20 | |
Specific heat | 0.44 | 0.461 | 0.494 | 0.5 | 0.5 | ||
J/g.℃ | |||||||
Thermal conductivity | 60.3 | 45.2 | 45.2 | 43.8 | 43.8 | ||
KJ/m.h℃ | |||||||
Coefficient of lines expansion | 18 | 17 | 17 | 19 | 19 | ||
a×10-6/ | |||||||
(20~1000℃) | |||||||
Micrographic structure | Austenite | Austenite | Austenite | Austenite | Austenite | ||
Magnetic properties | Nonmagnetic | Nonmagnetic | Nonmagnetic | Weak magnetic | Weak magnetic |
![]() | ||
![]() | ||
![]() | ||
![]() | ||
![]() |